nickel and cobalt base dental alloys

nickel and cobalt base dental alloys

( Negotiable )

|

Minimum Order

Localit:

-

Prix de commande minimale:

-

Commande minimale:

10 Kilogram

Packaging Detail:

polyethylene bags and wooden boxes

Delivery Time:

2-3 days

Supplying Ability:

500 Kilogram per Month

Payment Type:

T/T

Contacter maintenant

SINTAL MM Ltd

Bulgaria

Membre gratuit

Personne à contacter Mr. Dimitar

Zona B5, Bl.10, Sofia, Sofia district

Contacter maintenant

Description

Use: NiCrMo bonding alloy compatible with conventional ceramic materials with appropriate CTE range.
Melting Torch, Induction (HF), Light arc.
Casting time point: as soon as the molten mass begins to split (HF);
after complete melting of the pellet and obtaining а vibrating mirror surface surface (flame melting).
Pressure casting **0 **0 mbar.
Welding possible using methods such as laser welding and TIG impulse welding.
Additive material NiCr welding wire.
Pre-soldering NiCr-Sold Marranium.
Sand blasting: Use the available laboratory technique and the traditional way of processing.
Oxidation: optional.
Recommended ceramics: with suitable CTE ceramic range.
Cooling of ceramics: regular cooling, unless otherwise in the furnace recommended by the ceramic manufacturer.
Safety measures:
Despite this alloy does not contain toxic components as Be,  inhalation of metal vapor or dust  during casting and mechanical treatment should be avoided. Use aspiration! Observe the rules of hygienic work!

For professional use only!
Use: CoCrMo bonding alloy compatible with conventional ceramic materials with appropriate CTE range.
Melting Torch, Induction (HF), Light arc.
Casting time point: as soon as the molten mass begins to split (HF);
after complete melting of the pellet and obtainingаvibrating mirror surface (flame melting).
Pressure casting **0 **0 mbar.
Welding possible using methods such as laser welding and TIG impulse welding.
Additive material CoCr welding wire.
Pre-soldering CoCr-Sold Marranium
Sandblasting: Usetheavailable laboratory techniqueand the traditionalwayof processing.
Oxidation: optional.
Recommended Ceramics: with suitable CTE ceramic range.
Cooling of ceramics: regular cooling, unless otherwise in the furnace recommended by the ceramic manufacturer.
 
Safety measures:
Despite this alloy does not contain toxic components asBe,  inhalation of metal vapor or dust during casting and mechanical treatment should be avoided. Use aspiration!Observetherules of hygienicwork!
 
 
For professional use only!


 