Prix FOB
Obtenir le dernier prix15 ~ 20 USD / Kilohertz ( Negotiable )
|1 Kilogram Minimum Order
Pays:
China
N ° de modèle:
GB/T 2965-2007
Prix FOB:
15 ~ 20 USD / Kilohertz ( Negotiable )Obtenir le dernier prix
Localité:
baoji
Prix de commande minimale:
15 per Kilohertz
Commande minimale:
1 Kilogram
Packaging Detail:
wooden case
Heure de livraison:
15days
Capacité de Fournir:
100 Kilogram per Week
Payment Type:
T/T, L/C, D/A, D/P, PayPal, Other
Groupe de produits :
Personne àcontacter james
Yintai, Shaanxi
Generally, the manufacturing methods of composite steel plate
include: filling metal ingot rolling method, explosion compounding
method, rolling compression method, surfacing method, etc.
Considering the characteristics of titanium industry often USES
explosion after legal or rolling pressure connection, while the
actual production methods include (1) explosion after legal,
rolling pressure connection, including (2) (3) with the method of
continuous hot rolling plate rolling method. It is usually carried
out at room temperature, and the rolling pressure method is to
assemble and heat the plate.
Explosion restoration
The main point of the explosion: first, keep a certain space
between the two sheets of metal that you want to press, and then
put an appropriate amount of explosives on it. Detonating at one
end of the explosive, the explosion velocity is thousands of meters
per second, and the explosion can impact the titanium plate from
the Angle of the steel plate. In the collision point base material
plate and titanium plate because of the very large deformation
velocity and shows the fluid under ultra-high pressure, two metal
oxide film, gas adsorption layer on the surface of the rule out as
metal flow, clean surface and surface junction between the
instantaneous, called cold joint.
The titanium steel composite plate made by this method can continue
hot rolling to the plate thickness of 4mm, so it is also known as
the explosion recovery method.
Thick plate rolling method.
The thick plate rolling method initially put the titanium plate
(composite) and steel sheet (base material) into the embedded slab
assembly. At this time, between the titanium plate and the steel
between the appropriate intermediate embedded material, and in the
high vacuum of the electron beam welding. Finally, when the heating
furnace is heated, the required thickness is pressed on the thick
plate rolling mill, so that the titanium plate and the steel plate
are actually connected. Finally, the peripheral cutting is
separated into two plates.
Continuous hot rolling
Continuous hot rolling method and thick plate rolling method are
basically the same, the difference is two middle join is steel
plate, arc welding, under the atmosphere at last on the continuous
hot rolling mill continuous pad to the required thickness, in the
form of coil. Finally, the peripheral cutting is separated into two
plates.
Pays: | China |
N ° de modèle: | GB/T 2965-2007 |
Prix FOB: | 15 ~ 20 / Kilohertz ( Negotiable ) Obtenir le dernier prix |
Localité: | baoji |
Prix de commande minimale: | 15 per Kilohertz |
Commande minimale: | 1 Kilogram |
Packaging Detail: | wooden case |
Heure de livraison: | 15days |
Capacité de Fournir: | 100 Kilogram per Week |
Payment Type: | T/T, L/C, D/A, D/P, PayPal, Other |
Groupe de produits : | plate |