Photoresist Anti Etching Ink for Stainless Steel, Copper, Aluminum, Brass, By Vitayon Fine Chemical Industry Co., Ltd.(Shenzhen),
Pas encore membre de TradeKey.com? Inscrivez-vous pour vous connecter avec 9 millions d'importateurs et exportateurs. Rejoignez-le maintenant c'est gratuit |
BOOK A CALL
Book Call On Your Favorite Time

By Signing Up. I agree to TradeKey.com Terms of Use, Privacy Policy, IPR and receive emails related to our services

Contact Us
product
Prev
Photoresist Anti Etching Ink for Stainless Steel, Copper, Aluminum, Brass,
Next

Photoresist Anti Etching Ink for Stainless Steel, Copper, Aluminum, Brass,

( Negotiable )

|

5 Kilogram Minimum Order

Pays:

China

N ° de modèle:

-

Prix FOB:

( Negotiable ) Obtenir le dernier prix

Localité:

-

Prix de commande minimale:

-

Commande minimale:

5 Kilogram

Packaging Detail:

Black barrel

Heure de livraison:

3-10days after payment

Capacité de Fournir:

60 Kilogram per Month

Payment Type:

T/T, Western Union, Money Gram

Groupe de produits :

Contacter maintenant
Membre gratuit

Personne à contacter Dora

Shenzhen, Guangdong

Contacter maintenant

Spécification du produit

  • Usage: Electronics Chemicals
  • Brand Name: Vitayon

La description

Operation: Printing*-Pre-baking*-exposure*-developing*-post baking*-etching*-stripping(remove the ink)

Operation Detail:
1. Pre-treatment: Clean up the surface of material, remove the oil, wax, etc;
2. Adjust: It is ok to add some dilution to adjust the viscosity of ink(In spraying way, add dilution with 1 ink: 0.7 dilution), test the viscosity before applying, the percentage can not be over **0%;
3. Coating: If you use spraying way, the viscosity of ink should be ****0s; If you use screen printing way, please use *7T***0T mesh; The thickness of ink film should be over *5um. If you screen print a pattern, please turn to Step7 directly;
4. Pre-baking: Hot wind cycling drying with ****0degree, ****0 min, after it cools down, the ink won't stick to your hand, that will be ok;
5. Exposure: The exposure power should be ******0mj/cm2;
6. Developing: Wash it with 0.8%*1% Na2CO3 solvant, the power should be 2KG/ cm² , temperature should be *0degree± 2;
7. Post-baking: Hot wind cycling drying with **0degree, ****0min; It is better to expose them with exposure machine for **5min so that the etching resistant ability will be better;
8. Anti etching operation, if the anti etching ability is not strong, and the ink drops down, then you could extend the ink thickness and baking time;
9. Stripping: **8% NaOH solvant, ****0degree, ****0min( if the thickness of ink thicker, then the second baking time will be longer, so will the stripping time.

Pays: China
N ° de modèle: -
Prix FOB: ( Negotiable ) Obtenir le dernier prix
Localité: -
Prix de commande minimale: -
Commande minimale: 5 Kilogram
Packaging Detail: Black barrel
Heure de livraison: 3-10days after payment
Capacité de Fournir: 60 Kilogram per Month
Payment Type: T/T, Western Union, Money Gram
Groupe de produits : Functional coating

Send a direct inquiry to this supplier

To:

Dora < Vitayon Fine Chemical Industry Co., Ltd.(Shenzhen) >

Je veux savoir: