pad printing silicone rubber By Shenzhen Hong Ye Jie Technology Co., Ltd.,
Pas encore membre de TradeKey.com? Inscrivez-vous pour vous connecter avec 9 millions d'importateurs et exportateurs. Rejoignez-le maintenant c'est gratuit |
BOOK A CALL
Book Call On Your Favorite Time
Code
🗘

By Signing Up. I agree to TradeKey.com Terms of Use, Privacy Policy, IPR and receive emails related to our services

Contact Us
product
Prev
pad printing silicone rubber
Next

pad printing silicone rubber

7.8 ~ 15.9 USD / Kilogram ( Negotiable )

|

100 Kilogram Minimum Order

Pays:

China

N ° de modèle:

pad printing silicone rubber

Prix FOB:

7.8 ~ 15.9 USD / Kilogram ( Negotiable ) Obtenir le dernier prix

Localité:

China

Prix de commande minimale:

7.8 per Kilogram

Commande minimale:

100 Kilogram

Packaging Detail:

-

Heure de livraison:

Within 3 days after payment confirmed in our bank.

Capacité de Fournir:

5 Ton per Day

Payment Type:

L/C, T/T

Groupe de produits :

-

Contacter maintenant
Membre gratuit

Personne à contacter Ms. Tingting

Building A, No.3, Hongling First Road, Liulian Shibi, Pingdi Street, Longgang, Shenzhen, Guangdong,, Shenzhen, Guangdong

Contacter maintenant

Spécification du produit

  • Other Names: pad printing silicone rubber
  • Purity (%): 100%
  • Type: Adsorbent
  • Brand Name: hongyejie silicone

La description

Usages of pad Printing Silicon Rubber:
 
Pad printing silicone rubber is mainly use for printing irregular patterns of plastic toys, electroplating toys and trade makers . Pad printing silicone rubber as a carrier which transfer patterns on the steel plate to the toys products surface.
 
 
Features of Pad Printing Silicon Rubber:
 
Pad printing silicone rubber with high print times and abrasion resistance. Pad printing silicone rubber has good printing effects, permanent and durable. We can provide all kinds of color and our catalyst is free. 
 
 
 
Instructions of Pad Printing Silicon Rubber:
 
Pad printing silicone rubber is two-component silicone, part A is liquid silicon rubber, part B is catalyst. The usual mixture of silicone rubber and catalyst is **0: 2 or **0: 3. E.g. we take **0g of liquid silicon rubber and 2g*3g catalyst, mix them and pour it to your mold. A fter **4 hours, you will get a Pad printing silicone rubber.
 
Why the silicon pad is non-durable?
A This problem is caused not by the liquid silicon rubber itself, but in the process of filtering, the filtering handled not properly and impurities are not all filtered out; or in the process of packing as containers not cleaned thoroughly.
B As the silicon oil will break the molecular chain of the silicon rubber. More silicon oil added, softer the pad printing will be, meanwhile nondurable and easy ageing it will also turn to be.
C Some customers do not know well about the performance of silicon rubber. Actually, the durability of printing pad is closely related to the size of printing pattern. Some factories do not want to take the trouble to change the printing pad. While in fact, for large pattern, large silicone pads should be used, otherwise, use small one.(Generally, the ratio of the silicone pad to printing pattern is 3:1)
 
 
 
For getting further information about pad printing silicone rubber, PLS contact with Miss Nancy
TEL: ***6.************3 or
Mobile: ***************4
Email¼šhyr(at)szrl(dot)net
Website :w
Usages of pad Printing Silicon Rubber:
 
Pad printing silicone rubber is mainly use for printing irregular patterns of plastic toys, electroplating toys and trade makers . Pad printing silicone rubber as a carrier which transfer patterns on the steel plate to the toys products surface.
 
 
Features of Pad Printing Silicon Rubber:
 
Pad printing silicone rubber with high print times and abrasion resistance. Pad printing silicone rubber has good printing effects, permanent and durable. We can provide all kinds of color and our catalyst is free. 
 
 
 
Instructions of Pad Printing Silicon Rubber:
 
Pad printing silicone rubber is two-component silicone, part A is liquid silicon rubber, part B is catalyst. The usual mixture of silicone rubber and catalyst is **0: 2 or **0: 3. E.g. we take **0g of liquid silicon rubber and 2g*3g catalyst, mix them and pour it to your mold. A fter **4 hours, you will get a Pad printing silicone rubber.
 
Why the silicon pad is non-durable?
A This problem is caused not by the liquid silicon rubber itself, but in the process of filtering, the filtering handled not properly and impurities are not all filtered out; or in the process of packing as containers not cleaned thoroughly.
B As the silicon oil will break the molecular chain of the silicon rubber. More silicon oil added, softer the pad printing will be, meanwhile nondurable and easy ageing it will also turn to be.
C Some customers do not know well about the performance of silicon rubber. Actually, the durability of printing pad is closely related to the size of printing pattern. Some factories do not want to take the trouble to change the printing pad. While in fact, for large pattern, large silicone pads should be used, otherwise, use small one.(Generally, the ratio of the silicone pad to printing pattern is 3:1)
 
 
 
For getting further information about pad printing silicone rubber, PLS contact with Miss Nancy
TEL: ***6.************3 or
Mobile: ***************4

Pays: China
N ° de modèle: pad printing silicone rubber
Prix FOB: 7.8 ~ 15.9 / Kilogram ( Negotiable ) Obtenir le dernier prix
Localité: China
Prix de commande minimale: 7.8 per Kilogram
Commande minimale: 100 Kilogram
Packaging Detail: -
Heure de livraison: Within 3 days after payment confirmed in our bank.
Capacité de Fournir: 5 Ton per Day
Payment Type: L/C, T/T
Groupe de produits : -

Send a direct inquiry to this supplier

To:

Ms. Tingting < Shenzhen Hong Ye Jie Technology Co., Ltd. >

Je veux savoir: