Master alloy for goldsmith's, Suitable for 9/10/14K in yellow gold
Next

Master alloy for goldsmith's, Suitable for 9/10/14K in yellow gold

200 ~ 270 USD / Kilogram ( Negotiable )

|

1 Kilogram Minimum Order

Pays:

China

N ° de modèle:

GYS10

Prix FOB:

200 ~ 270 USD / Kilogram ( Negotiable ) Obtenir le dernier prix

Localité:

China

Prix de commande minimale:

200 per Kilogram

Commande minimale:

1 Kilogram

Packaging Detail:

Plastic bottle in carton

Heure de livraison:

within 3 days

Capacité de Fournir:

6000 Kilogram per Year

Payment Type:

Money Gram, Western Union, T/T

Groupe de produits :

Contacter maintenant
Membre gratuit

Personne à contacter Tony

No1. GuangXing Road, DaYan Industrial Park, HuangPu Town, Zhongshan, Guangdong

Contacter maintenant

Spécification du produit

  • yellow color:USD 230

La description


Application
Karat 9/*0/*4K Color Hamilton Yellow
Application C, C/S Special High fluidity
Composition *0% Ag    
 
Color
karat L * a *   b *
9K *0.*8 2.*7 *9.*6
*0K *9.*4 3.*1 *9.*0
*4K *9.*6 3.*9 *9.*1
   
Characteristics
  Density [g/cm^3] Hardness [HV]   Melting range [° C]
9K *0.*8 **3 ******4
*0K *1.*6 **6 ******9
*4K *2.*4 **2 ******2
 
Castingtemperature: Suggesttemperature: *******0° C
F lasks temperature: Suggest temperature: ******0° C
Help-solvent: Suggest using borax as help-solvent, for casting by machine don’ t need it.
Set down casting temperatureaccording to the identity of product, lower flasks temperature for layer product; higher flasks temperature for lighter product.
Suggest advance-melting before casting, and make sure melting well-proportioned.
 
 
Water Cooling
Cooling in the air for ****0 minutes before water cooling, more cooling time in the air for the layer product.
 
Cleaning
Using high pressure water to cleaning the plaster, and than put the product into ***0% hydrofluoric acid in order to cleaning the residual plaster.
 
Backup
C=Casting    C/S=Casting with stones 

Pays: China
N ° de modèle: GYS10
Prix FOB: 200 ~ 270 / Kilogram ( Negotiable ) Obtenir le dernier prix
Localité: China
Prix de commande minimale: 200 per Kilogram
Commande minimale: 1 Kilogram
Packaging Detail: Plastic bottle in carton
Heure de livraison: within 3 days
Capacité de Fournir: 6000 Kilogram per Year
Payment Type: Money Gram, Western Union, T/T
Groupe de produits : yellow gold alloy series

Send a direct inquiry to this supplier

To:

Tony < ZhongShan Jia Rui Te Noble Metal Materials Co., Ltd >

Je veux savoir: